By combining 3 to 4 polyamide building components Co-Polyamides with melting ranges between 80~140°C can be produced. Due to the very good resistance against solvents used in dry cleaning, Kola™ Co-PA are perfect to be used in the garment industry. Co-Polyamides can be divided in groups for different bonding temperatures as: 90~100 °C for leather garments, 100~130°C for garments, 130~150°C for uniforms and shirts, technical applications. |
|
|
|
|